Abstract
We computationally investigate fabrication tolerances in negative-curvature antiresonant tube-lattice fibers. Since the dominant loss mechanisms for silica in the mid-infrared (mid-IR) is material absorption, , which offers a reduced loss over that wavelength range, is a natural candidate for mid-IR antiresonant fibers. However, any fiber fabrication technology, including for soft glasses, will have imperfections. Therefore, it is important to know how imperfect fabrication will affect the results of a fiber design. We study perturbations to the fiber, including a nonconstant tube-wall thickness, a single cladding tube with a different radius, a single cladding tube with a different tube-wall thickness, and “key” sections in the jacket.
© 2016 Optical Society of America
Full Article | PDF ArticleMore Like This
Md Imran Hasan, Nail Akhmediev, and Wonkeun Chang
Opt. Lett. 42(4) 703-706 (2017)
Amy Van Newkirk, J. E. Antonio-Lopez, James Anderson, Roberto Alvarez-Aguirre, Zeinab Sanjabi Eznaveh, Gisela Lopez-Galmiche, Rodrigo Amezcua-Correa, and Axel Schülzgen
Opt. Lett. 41(14) 3277-3280 (2016)
Jerome Lapointe, Yannick Ledemi, Sébastien Loranger, Victor Lambin Iezzi, Elton Soares de Lima Filho, Francois Parent, Steeve Morency, Younes Messaddeq, and Raman Kashyap
Opt. Lett. 41(2) 203-206 (2016)